| d | dp | z2 | z1 | d2 max | d2 min |
|---|
| M6 | 4.5000 | 6.0000 | 2.5000 | 4.0000 | 3.9000 |
| M8 | 6.0000 | 7.5000 | 3.0000 | 5.4000 | 5.3000 |
| M10 | 8.0000 | 9.0000 | 4.5000 | 7.2000 | 7.1000 |
| M12 | 8.0000 | 10.0000 | 4.5000 | 7.2000 | 7.1000 |
| M16 | 12.0000 | 12.0000 | 5.0000 | 11.0000 | 10.9000 |
| M20 | 15.5000 | 14.0000 | 5.5000 | 14.4000 | 14.3000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Grade-5.8 Hard-End |
|---|
| Standard Number | DIN6332 |
|---|
| Second Standard | - |
|---|
| Drive | Hexagonsocket |
|---|
| Head | NON |
|---|
| American Generic Brand Term | ALLEN,GRUB |
|---|
| Diameter | ?6,?8,?10,?12,?16,?20 |
|---|
| Length | 30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150 |
|---|