Metric Coarse Socket Set Screw Cone Point Stainless-Steel-A2 DIN914

SKU: 1735
Details
Details
Metric Coarse Socket Set Screw Cone Point Stainless-Steel-A2 DIN914
d1dt maxtse
M1.40.35000.60000.70000.7720
M1.60.40000.70000.70000.7720
M1.80.45000.80000.70000.7720
M20.50000.80000.90000.9920
M2.50.65001.20001.30001.4330
M30.75001.20001.50001.6530
M41.00001.50002.00002.2050
M51.25002.00002.50002.7560
M61.50002.00003.00003.3070
M82.00003.00004.00004.4090
M102.50006.00005.00005.5120
M123.00008.00006.00006.6140
M143.50009.00006.00006.6140
M164.000010.00008.00008.8180
M184.500011.000010.000011.0230
M205.000012.000010.000011.0230
M225.500013.600012.000013.2280
M246.000015.000012.000013.2280
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN914
Second StandardISO4027,BS4168
DriveHexagonsocket
HeadNON
American Generic Brand TermALLEN,GRUB
Diameter M2,M2.5,M3,M4,M5,M6,M8,M10,M12,M14,M16,M18,M20