BSW Whitworth Socket Set Screw Flat Point Grade-14.9-45H BS2470

SKU: 1765
Details
Details
BSW Whitworth Socket Set Screw Flat Point Grade-14.9-45H BS2470
Dds nomt mindp maxdp ming maxg min
3/16”0.18753/32”0.07500.12700.12000.04900.0410
1/4”0.25001/8”0.10000.15600.14900.06700.0590
5/16”0.31255/32”0.12500.20300.19500.08200.0740
3/8”0.37503/16”0.15000.25000.24100.09900.0890
7/16”0.43757/32”0.17500.29700.28700.11400.1040
1/2”0.50001/4”0.20000.34400.33400.13000.1200
5/8”0.62505/16”0.25000.46900.45600.16400.1480
3/4”0.75003/8”0.30000.56200.54900.19600.1800
7/8”0.87501/2”0.40000.65600.64200.22700.2110
1”1.00009/16”0.45000.75000.73400.26000.2400
Additional Info
Additional Info
Weight0.0000
MaterialGrade-14.9-45H
Standard NumberBS2470
Second Standard-
DriveHexagonsocket
HeadNON
American Generic Brand TermALLEN,GRUB
Diameter 3/16”,1/4”,5/16”,3/8”,7/16”,1/2”,5/8”,3/4”,7/8”,1”
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3."