BA Socket Set Screw Cup Point Grade-14.9-45H BS2470
SKU:
1771
Details
Details
BA Socket Set Screw Cup Point Grade-14.9-45H BS2470
D | s nom | t min | dp max |
---|
8BA | 0.0350 | 0.3000 | 0.0470 |
6BA | 0.0500 | 0.0400 | 0.0610 |
5BA | 1/16" | 0.0500 | 0.0670 |
4BA | 1/16" | 0.0500 | 0.0740 |
3BA | 5/64" | 0.0620 | 0.0870 |
2BA | 3/32" | 0.0750 | 0.1020 |
1BA | 3/32" | 0.0750 | 0.1150 |
OBA | 1/8" | 0.1000 | 0.1320 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-14.9-45H |
---|
Standard Number | BS2470 |
---|
Second Standard | - |
---|
Drive | Hexagonsocket |
---|
Head | NON |
---|
American Generic Brand Term | ALLEN,GRUB |
---|
Diameter | 8BA,6BA,5BA,4BA,3BA,2BA,1BA,OBA |
---|
Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3." |
---|