| D | d max | d min | dk min | k ref | s nom | y min |
|---|---|---|---|---|---|---|
| No.0 | 0.0600 | 0.0568 | 0.1170 | 0.0440 | 0.0350 | 0.0250 |
| No.1 | 0.0730 | 0.0695 | 0.1430 | 0.0540 | 0.0500 | 0.0310 |
| No.2 | 0.0860 | 0.0822 | 0.1680 | 0.0640 | 0.0500 | 0.0380 |
| No.3 | 0.0990 | 0.0949 | 0.1930 | 0.0730 | 1/16" | 0.0440 |
| No.4 | 0.1120 | 0.1075 | 0.2180 | 0.0830 | 1/16" | 0.0550 |
| No.5 | 0.1250 | 0.1202 | 0.2400 | 0.0900 | 5/64" | 0.0360 |
| No.6 | 0.1380 | 0.1329 | 0.2630 | 0.0970 | 5/64" | 0.0660 |
| No.8 | 0.1640 | 0.1585 | 0.3110 | 0.1120 | 3/32" | 0.0760 |
| No.10 | 0.1900 | 0.1840 | 0.3590 | 0.1270 | 1/8" | 0.0870 |
| 1/4" | 0.2500 | 0.2435 | 0.4800 | 0.1610 | 5/32" | 0.1110 |
| 5/16" | 0.3125 | 0.3053 | 0.6000 | 0.1980 | 3/16" | 0.1350 |
| 3/8" | 0.3750 | 0.3678 | 0.7200 | 0.2340 | 7/32" | 0.1590 |
| 7/16" | 0.4375 | 0.4294 | 0.7810 | 0.2340 | 1/4" | 0.1590 |
| 1/2" | 0.5000 | 0.4919 | 0.8720 | 0.2510 | 5/16" | 0.1720 |
| 5/8" | 0.6250 | 0.6163 | 1.1120 | 0.3240 | 3/8" | 0.2200 |
| 3/4" | 0.7500 | 0.7406 | 1.3550 | 0.3960 | 1/2" | 0.2200 |
| 7/8" | 0.8750 | 0.8647 | 1.6040 | 0.4680 | 9/16" | 0.2480 |
| 1" | 1.0000 | 0.9886 | 1.8410 | 0.5400 | 5/8" | 0.2970 |
| 1.1/8" | 1.1250 | 1.1086 | 2.0790 | 0.6110 | 3/4" | 0.3250 |
| 1.1/4" | 1.2500 | 1.2336 | 2.3160 | 0.6830 | 7/8" | 0.3580 |
| 1.3/8" | 1.3750 | 1.3566 | 2.5530 | 0.7550 | 7/8" | 0.4020 |
| 1.1/2" | 1.5000 | 1.4818 | 2.7910 | 0.8270 | 1." | 0.4350 |
| Weight | 0.0000 |
|---|---|
| Material | Phospher-Bronze |
| Standard Number | B18.3 |
| Second Standard | BS2470 |
| Drive | Hexagonsocket |
| Head | COUNTERSUNK |
| American Generic Brand Term | FLAT,SPLINE |
| Diameter | No.0,No.1,No.2,No.3,No.4,No.5,No.6,No.8,No.10,1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2" |
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",6.",8." |