UNF Socket Countersunk Screw Nylon-66 B18.3

SKU: 1710
Details
Details
UNF Socket Countersunk Screw Nylon-66 B18.3
Dd maxd mindk mink refs nomy min
No.00.06000.05680.11700.04400.03500.0250
No.10.07300.06950.14300.05400.05000.0310
No.20.08600.08220.16800.06400.05000.0380
No.30.09900.09490.19300.07301/16"0.0440
No.40.11200.10750.21800.08301/16"0.0550
No.50.12500.12020.24000.09005/64"0.0360
No.60.13800.13290.26300.09705/64"0.0660
No.80.16400.15850.31100.11203/32"0.0760
No.100.19000.18400.35900.12701/8"0.0870
1/4"0.25000.24350.48000.16105/32"0.1110
5/16"0.31250.30530.60000.19803/16"0.1350
3/8"0.37500.36780.72000.23407/32"0.1590
7/16"0.43750.42940.78100.23401/4"0.1590
1/2"0.50000.49190.87200.25105/16"0.1720
5/8"0.62500.61631.11200.32403/8"0.2200
3/4"0.75000.74061.35500.39601/2"0.2200
7/8"0.87500.86471.60400.46809/16"0.2480
1"1.00000.98861.84100.54005/8"0.2970
1.1/8"1.12501.10862.07900.61103/4"0.3250
1.1/4"1.25001.23362.31600.68307/8"0.3580
1.3/8"1.37501.35662.55300.75507/8"0.4020
1.1/2"1.50001.48182.79100.82701."0.4350
Additional Info
Additional Info
Weight0.0000
MaterialNylon-66
Standard NumberB18.3
Second StandardBS2470
DriveHexagonsocket
HeadCOUNTERSUNK
American Generic Brand TermFLAT,ALLEN
Diameter No.0,No.1,No.2,No.3,No.4,No.5,No.6,No.8,No.10,1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2"
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",6.",8."