BSW Whitworth Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470

SKU: 1713
Details
Details
BSW Whitworth Socket Countersunk Screw Stainless-Steel 18/8-304-A2 BS2470
Dd maxdk maxdk mink noms nomt min
3/16”0.18750.35600.31400.08703/32”0.0620
1/4”0.25000.47500.42000.11605/32”0.0790
5/16”0.31250.59400.52700.14603/16”0.0990
3/8”0.37500.71200.63500.17407/32”0.1130
7/16”0.43750.83100.74200.20401/4”0.1380
1/2”0.50000.95000.87000.23305/16”0.1620
5/8”0.62501.18701.06400.29103/8”0.2260
3/4”0.75001.42501.28000.34903/8”0.2670
7/8”0.87501.66201.52600.40701/2”0.3350
1”1.00001.90001.74500.46609/16”0.3940
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard NumberBS2470
Second Standard-
DriveHexagonsocket
HeadCOUNTERSUNK
American Generic Brand TermFLAT,ALLEN
Diameter 3/16”,1/4”,5/16”,3/8”,7/16”,1/2”,5/8”,3/4”,7/8”,1”
Length1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10