UNF Socket Cap Screw 1936 Stainless-Steel 18/8-304-A2 BS2470

SKU: 1641
Details
Details
UNF Socket Cap Screw 1936 Stainless-Steel 18/8-304-A2 BS2470
Dd maxd mindk maxdk mink maxk minc mins nomt minw minb min
No.00.06000.05680.09600.09100.06000.05700.05400.05000.02500.02000.5000
No.10.07300.06950.11800.11200.07300.07000.06600.05000.03100.02500.6250
No.20.08600.08220.14000.13400.08600.08300.07701/16"0.03800.02900.6250
No.30.09900.09490.16100.15400.09900.09500.08905/64"0.04400.03400.6250
No.40.11200.10750.18300.17600.11200.10800.10105/64"0.05100.03800.7500
No.50.12500.12020.20500.19800.12500.12100.11203/32"0.05700.04300.7500
No.60.13800.13290.22600.21800.13800.13400.12403/32"0.06400.04700.7500
No.80.16400.15850.27000.26200.16400.15900.14801/8"0.07700.05600.8750
No.100.19000.18400.31200.30300.19000.18500.17105/32"0.09000.06500.8750
1/4"0.25000.24350.37500.36500.25000.24400.22503/16"0.12000.09501.0000
5/16"0.31250.30530.43700.42500.31200.30600.28107/32"0.15100.11901.1250
3/8"0.37500.36780.56200.55000.37500.36800.33705/16"0.18200.14301.2500
7/16"0.43750.42940.62500.61100.43700.43000.39405/16"0.21300.16601.3750
1/2"0.50000.49190.75000.73500.50000.49200.45003/8"0.24500.19001.5000
5/8"0.62500.61630.87500.85800.62500.61600.56201/2"0.30700.23801.7500
3/4"0.75000.74061.00000.98200.75000.74000.67509/16"0.37000.28502.0000
7/8"0.87500.86471.12501.10500.87500.86400.78709/16"0.43200.33302.2500
1"1.00000.98861.31201.29101.00000.98800.90005/8"0.49500.38002.5000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard NumberBS2470
Second Standard-
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN
Diameter No.0,No.1,No.2,No.3,No.4,No.5,No.6,No.8,No.10,1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1"
Length1/16",1/8",5/32",3/16",7/32",1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8."