D s dk Max dk Min k Max k Min t b
M1.41.30002.74002.46001.40001.26000.600014.0000
M1.61.50003.14002.86001.60001.46000.700015.0000
M21.50003.98003.62002.00001.87601.000016.0000
M2.52.00004.68004.32002.50002.36001.100017.0000
M32.50005.68005.32003.00002.86001.300018.0000
M43.00007.22006.78004.00003.82002.000020.0000
M54.00008.72008.28005.00004.82002.500022.0000
M65.000010.22009.78006.00005.70003.000024.0000
M86.000013.270012.73008.00007.64004.000028.0000
M108.000016.000016.270010.00009.64005.000032.0000
M1210.000018.000018.270012.000011.57006.000036.0000
M1412.000021.000021.330014.000013.57007.000040.0000
M1614.000024.000024.330016.000015.57008.000044.0000
M1814.000027.000027.330018.000017.57009.000048.0000
M2017.000030.000030.330020.000019.480010.000052.0000
M2217.000033.000033.390022.000021.480011.000056.0000
M2419.000036.000036.390024.000023.480012.000060.0000
M2719.000040.000040.390027.000026.480013.200066.0000
M3022.000045.000045.390030.000029.480015.500072.0000
M3324.000050.390049.610033.000032.380018.000078.0000
M3627.000054.460053.540036.000035.380019.000084.0000
M4232.000063.460062.540042.000041.368024.000096.0000
M4836.000072.460071.540048.000047.380028.0000108.0000
M5641.000084.540083.460056.000056.260034.0000124.0000
M6446.000096.540095.460064.000063.260038.0000140.0000
M7255.0000108.5400107.460072.000071.260043.0000156.0000
M8065.0000120.5400119.460080.000079.260048.0000172.0000
M9075.0000135.6300134.370090.000089.130054.0000192.0000
M10085.0000150.6300149.3700100.000099.130060.0000212.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberDIN912
Second StandardBS4168,ISO4762
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52,M56,M60,M64,M68,M72,M76,M80,M90,M100,M110,M125,M140,M160
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400,420,440,460,480,500
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.