BA Socket Cap Screw Stainless-Steel 18/8-304-A2 BS2470

SKU: 1653
Details
Details
BA Socket Cap Screw Stainless-Steel 18/8-304-A2 BS2470
D d max d min a max a min k max k min c min s nom t min w min b min
8BA0.08660.08230.14000.13300.08700.08300.0860 1/16"0.04300.03200.7500
6BA0.11020.10570.18700.18000.11000.10600.0990 5/64"0.05000.03700.7500
5BA0.12600.12120.21900.21100.12600.12200.1130 3/32"0.05800.04300.7500
4BA0.14170.13660.21900.21100.14200.13700.1280 3/32"0.06600.04800.7500
3BA0.16140.15590.25000.24200.16100.15600.1450 1/8"0.07500.05500.8750
2BA0.18500.17900.31200.30300.18700.18200.1680 5/32"0.08900.06300.8750
1BA0.20870.20270.31200.30300.20900.20400.1880 5/32"0.10000.07101.0000
0BA0.23620.22970.37500.36500.23600.23000.2120 3/16"0.11300.08001.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard NumberBS2470
Second Standard-
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN
Diameter 0BA,2BA,3BA,4BA,6BA,8BA
Length1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3