UNF Socket Button Head Screw Brass B18.3

SKU: 1676
Details
Details

UNF Socket Button Head Screw Brass B18.3

dda maxa minh maxh minsj nomy minf maxf min
No.00.06000.11400.10400.03200.02600.01000.03500.02000.01000.0050
No.10.07300.13900.12900.03900.03300.01000.05000.02800.01000.0050
No.20.08600.16400.15400.04600.03800.01000.05000.02800.01000.0050
No.30.09900.18800.17600.05200.04400.01001/16"0.03500.01000.0050
No.40.11200.21300.20100.05900.05100.01501/16"0.03500.01000.0050
No.50.12500.23800.22600.06600.05800.01505/64"0.04400.01000.0050
No.60.13800.26200.25000.07300.06300.01505/64"0.04400.01000.0050
No.80.16400.31200.29800.08700.07700.01503/32"0.05200.01500.0100
No.100.19000.36100.34700.10100.09100.02001/8"0.07000.01500.0100
1/4"0.25000.43700.41900.13200.12200.03105/32"0.08700.02000.0150
5/16"0.31250.54700.52700.16600.15200.03103/16"0.10500.02000.0150
3/8"0.37500.65600.63600.19900.18500.03107/32"0.12200.02000.0150
1/2"0.50000.87500.85100.26500.24500.04605/16"0.17500.03000.0200
5/8"0.62501.00000.97000.33100.31100.06203/8"0.21000.03000.0200

UNF Socket Button Head Screw Brass B 18.3

Additional Info
Additional Info
Weight0.0000
MaterialBRASS
Standard NumberB18.3
Second StandardBS2470
DriveHexagonsocket
HeadButtoncap
American Generic Brand TermALLEN
Diameter No.0,No.1,No.2,No.3,No.4,No.5,No.6,No.8,No.10,1/4",5/16",3/8",1/2",5/8"
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5."
Tags
Tags