BSF Socket Button Head Screw Stainless-Steel 18/8-304-A2

SKU: 1684
Details
Details
BSF Socket Button Head Screw Stainless-Steel 18/8-304-A2
ddk maxb max e max k max g maxr noms key t min
3/16"0.36100.18800.18600.10100.02000.21801/8"1.0000
1/4"0.43700.25000.23200.13200.03100.25405/32"1.0000
5/16"0.54700.31300.26800.16600.03100.31403/16"1.0000
3/8"0.65600.37500.30400.19900.03100.37307/32"1.2500
7/16"0.75000.43800.34000.23200.03100.41701/4"1.5000
1/2"0.87500.50000.41400.26500.04600.48605/16"2.0000
5/8"1.00000.62500.48600.33100.06200.52803/8"2.0000
3/4"1.21800.75000.61300.39800.07800.67001/2"2.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard Number.
Second Standard-
DriveHexagonsocket
HeadButtoncap
American Generic Brand TermALLEN
Diameter 3/16",1/4",5/16",3/8",7/16",1/2",5/8",3/4"
Length1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10
Tags