BA Socket Button Head Screw Stainless-Steel 18/8-304-A2
SKU:
1686
Details
Details
BA Socket Button Head Screw Stainless-Steel 18/8-304-A2
| D | k max | dk max | s nom | t min | d max |
|---|
| 8BA | 0.0460 | 0.1640 | 0.0500 | 0.0280 | 0.0870 |
| 6BA | 0.0590 | 0.2130 | 1/16" | 0.0350 | 0.1100 |
| 5BA | 0.0660 | 0.2380 | 5/64" | 0.0440 | 0.1260 |
| 4BA | 0.0730 | 0.2620 | 5/64" | 0.0440 | 0.1420 |
| 3BA | 0.0870 | 0.3120 | 3/32" | 0.0520 | 0.1610 |
| 2BA | 0.1010 | 0.3610 | 1/8" | 0.0700 | 0.1850 |
| 1BA | 0.1140 | 0.3950 | 1/8" | 0.0780 | 0.2090 |
| OBA | 0.1320 | 0.4370 | 5/32" | 0.0870 | 0.2360 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel 18/8-304-A2 |
|---|
| Standard Number | . |
|---|
| Second Standard | - |
|---|
| Drive | Hexagonsocket |
|---|
| Head | Buttoncap |
|---|
| American Generic Brand Term | ALLEN |
|---|
| Diameter | 0BA,2BA,3BA,4BA,6BA,8BA |
|---|
| Length | 1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3 |
|---|