Metric Coarse Slotted Grub (Set) Screw Cup Point Stainless-Steel-A2 DIN438

SKU: 1789
Details
Details
Metric Coarse Slotted Grub (Set) Screw Cup Point Stainless-Steel-A2 DIN438
dt minn mindz maxdz min
M1.60.56000.31000.80000.5500
M20.64000.31001.00000.7500
M2.50.72000.46001.20000.9500
M30.80000.46001.40001.1500
M3.50.96000.56001.70001.4500
M41.12000.66002.00001.7500
M51.28000.86002.50002.2500
M61.60001.06003.00002.7500
M82.00001.26005.00004.7000
M102.40001.66006.00005.7000
M122.80002.06008.00007.7000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN438
Second StandardISO7436
DriveSlot
HeadNON
American Generic Brand TermGRUB
Diameter M1.6,M1.8,M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10,M12
Length3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40