Metric Coarse Slotted Grub Screw with Dog Cone Point Grade-14.9-45H DIN926
SKU:
1784
Details
Details
Metric Coarse Slotted Grub Screw with Dog Cone Point Grade-14.9-45H DIN926
D | dp max | n min | t min |
---|
?1 | 0.5000 | 0.2000 | 0.4000 |
?1.2 | 0.7000 | 0.2000 | 0.4000 |
M1.4 | 0.8000 | 0.2000 | 0.4800 |
M1.6 | 0.8000 | 0.2500 | 0.5600 |
M2 | 1.2000 | 0.2500 | 0.6400 |
M2.5 | 1.5000 | 0.4000 | 0.7200 |
M3 | 2.0000 | 0.5000 | 0.8000 |
M3.5 | 2.5000 | 0.5000 | 0.9600 |
M4 | 2.8000 | 0.6000 | 1.1200 |
M5 | 3.5000 | 0.8000 | 1.2800 |
M6 | 4.5000 | 1.0000 | 1.6000 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | Grade-14.9-45H |
---|
Standard Number | DIN926 |
---|
Second Standard | - |
---|
Drive | Slot |
---|
Head | NON |
---|
American Generic Brand Term | GRUB |
---|
Diameter | ?1,?1.2,M1.4,M1.6,M2,M2.5,M3,M3.5,M4,M5,M6 |
---|
Length | 3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30 |
---|