Metric Coarse Hexagon Socket Shoulder Screw f9 Stainless-Steel-A2 ISO7379f9

SKU: 1778
Details
Details
Metric Coarse Hexagon Socket Shoulder Screw f9 Stainless-Steel-A2 ISO7379f9
D nom681012162024
D1M5M6M8M10M12M16M20
D f9 max5.99907.98709.987011.984015.984019.980023.9800
D f9 min5.96007.95109.951011.941015.941019.928023.9280
A max10.000013.000016.000018.000024.000030.000036.0000
A min9.780012.730015.730017.730023.670029.670035.6100
H max4.50005.50007.00009.000011.000014.000016.0000
H min4.32005.32006.78008.780010.730013.730015.7300
S max0.60000.80001.00001.20001.60002.00002.4000
J3.00004.00005.00006.00008.000010.000012.0000
T2.40003.30004.20004.90006.60008.800010.0000
K min5.42007.42009.420011.420015.420019.420024.4200
F max2.50002.50002.50002.50002.50002.50003.0000
G max3.86004.58006.25007.91009.570013.230016.5700
G min3.68004.40006.03007.69009.350012.950016.3000
I max2.40002.60002.80003.00004.00004.80005.6000
N max0.66000.69000.80000.93001.03001.30001.4600
N min0.50000.53000.64000.77000.87001.14001.3000
E max9.750011.250013.250016.400018.400022.400027.4000
M max7.50009.200011.200015.200018.200022.400027.4000
R min0.20000.40000.40000.60000.60000.80000.8000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberISO7379f9
Second StandardDIN9841
DriveHexagonsocket
HeadCAP
American Generic Brand TermALLEN,STRIPPER
Diameter M5,M6,M8,M10,M12,M14,M16,M18,M20,M22,M24
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.