Metric Fine Socket Button Head Screw Grade-10.9 ISO7380

SKU: 1665
Details
Details

Metric Fine Socket Button Head Screw Grade-10.9 ISO7380


D        dk             k                  t                      s              
M23.70001.30000.70001.2500
M2.54.35001.40000.85001.5000
M35.70001.65001.04002.0000
M47.60002.20001.30002.5000
M59.50002.75001.56003.0000
M610.50003.30002.08004.0000
M814.00004.40002.60005.0000
M1017.50005.50003.12006.0000
M1221.00006.60004.16008.0000
M1628.00008.80005.200010.0000

 

 

Metric Fine thread Socket allen  Button Head Screw Grade-10.9 ISO7380 iso 7380

Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberISO7380
Second StandardBS4168
DriveHexagonsocket
HeadButton
American Generic Brand TermALLEN
Diameter M6(0.75p),M8(1.00p),M10(1.00p),M10(1.25p),M12(1.25p),M12(1.50p),M14(1.50p),M16(1.50p)
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.