BA Socket Set Screw Cup Point Grade-14.9-45H BS2470
SKU:
1771
Details
Details
BA Socket Set Screw Cup Point Grade-14.9-45H BS2470
| D | s nom | t min | dp max |
|---|
| 8BA | 0.0350 | 0.3000 | 0.0470 |
| 6BA | 0.0500 | 0.0400 | 0.0610 |
| 5BA | 1/16" | 0.0500 | 0.0670 |
| 4BA | 1/16" | 0.0500 | 0.0740 |
| 3BA | 5/64" | 0.0620 | 0.0870 |
| 2BA | 3/32" | 0.0750 | 0.1020 |
| 1BA | 3/32" | 0.0750 | 0.1150 |
| OBA | 1/8" | 0.1000 | 0.1320 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Grade-14.9-45H |
|---|
| Standard Number | BS2470 |
|---|
| Second Standard | - |
|---|
| Drive | Hexagonsocket |
|---|
| Head | NON |
|---|
| American Generic Brand Term | ALLEN,GRUB |
|---|
| Diameter | 8BA,6BA,5BA,4BA,3BA,2BA,1BA,OBA |
|---|
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3." |
|---|