Dk maxds nomds maxds mindk nomdk maxdk minn nominaln maxn mint nomt maxt min
M1.60.96001.40001.60001.20003.00003.30002.70000.53000.60000.46000.73000.80000.6500
M21.20001.80002.00001.60003.80504.18003.43000.63000.70000.56000.90001.00000.8000
M2.51.50002.30002.50002.10004.70505.08004.33000.73000.80000.66001.10001.20001.0000
M31.65002.80003.00002.60005.60505.98005.23000.93001.00000.86001.32501.45001.2000
M3.51.93003.26003.50003.02006.50006.95006.05000.93001.00000.86001.55001.70001.4000
M42.20003.76004.00003.52007.50007.95007.05001.13001.20001.06001.75001.90001.6000
M4.52.35004.26004.50004.02008.30008.75007.85001.13001.20001.06001.95002.10001.8000
M52.50004.76005.00004.52009.20009.65008.75001.38501.51001.26002.15002.30002.0000
M5.52.75005.26005.50005.020010.200010.75009.65001.38501.51001.26002.35002.50002.2000
M63.00005.76006.00005.520011.000011.550010.45001.78501.91001.66002.60002.80002.4000
M73.50006.71007.00006.420012.500013.050011.95002.18502.31002.06003.00003.20002.8000
M84.00007.71008.00007.420014.500015.050013.95002.18502.31002.06003.45003.70003.2000
Additional Info
Additional Info
Weight0.0000
MaterialALUMINIUM
Standard NumberDIN95
Second StandardISO1210
DriveSlot
HeadRaisedcountersunk
American Generic Brand TermOVAL
Diameter M3,M3.5,M4,M4.5,M5,M5.5,M6,M7,M8
Length8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100