Metric Pozi Countersunk Wood Screw Steel DIN7997Z

SKU: 602
Details
Details
Metric Pozi Countersunk Wood Screw Steel DIN7997Z
ddkk maxl minl max
23.80001.20008.000020.0000
2.54.70001.500010.000020.0000
35.60001.650010.000040.0000
3.56.50001.930010.000045.0000
47.50002.200012.000060.0000
4.58.30002.350016.000060.0000
59.20002.500016.000080.0000
5.510.20002.750020.000080.0000
611.00003.000040.000080.0000
712.50003.500040.000080.0000
814.00004.000040.000080.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN7997Z
Second Standard-
DrivePOZI,CROSSRECESSED
HeadCOUNTERSUNK
American Generic Brand Term-
Diameter 2,2.5,3,3.5,4,4.5,5,5.5,6,7,8
Length8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80