Metric Hexagon Coach Screw Stainless-Steel-A4 DIN571

SKU: 620
Details
Details
Metric Hexagon Coach Screw Stainless-Steel-A4 DIN571
dsek nominalk maxk min
47.00007.70002.80003.10002.5000
58.00008.63003.50003.88003.1300
610.000010.89004.00004.38003.6300
712.000013.20005.00005.38004.6300
813.000014.20005.50005.88005.1300
1017.000018.72007.00007.45006.5500
1219.000020.88008.00008.45007.5500
1624.000026.170010.000010.45009.5500
2030.000033.000013.000013.900012.1000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A4
Standard NumberDIN571
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermLAG,WOOD
Diameter 4,5,6,7,8,10,12,16,20
Length16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300