| d | s | e | k nominal | k max | k min |
|---|---|---|---|---|---|
| 4 | 7.0000 | 7.7000 | 2.8000 | 3.1000 | 2.5000 |
| 5 | 8.0000 | 8.6300 | 3.5000 | 3.8800 | 3.1300 |
| 6 | 10.0000 | 10.8900 | 4.0000 | 4.3800 | 3.6300 |
| 7 | 12.0000 | 13.2000 | 5.0000 | 5.3800 | 4.6300 |
| 8 | 13.0000 | 14.2000 | 5.5000 | 5.8800 | 5.1300 |
| 10 | 17.0000 | 18.7200 | 7.0000 | 7.4500 | 6.5500 |
| 12 | 19.0000 | 20.8800 | 8.0000 | 8.4500 | 7.5500 |
| 16 | 24.0000 | 26.1700 | 10.0000 | 10.4500 | 9.5500 |
| 20 | 30.0000 | 33.0000 | 13.0000 | 13.9000 | 12.1000 |
| Weight | 0.0000 |
|---|---|
| Material | BRASS |
| Standard Number | DIN571 |
| Second Standard | - |
| Drive | Hexagon |
| Head | HEXAGON |
| American Generic Brand Term | LAG,WOOD |
| Diameter | 4,5,6,7,8,10,12,16,20 |
| Length | 16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300 |