Metric Coarse Knurled Round Head Thumb Screw Low Type Stainless-Steel-A1 DIN653

SKU: 565
Details
Details
Metric Coarse Knurled Round Head Thumb Screw Low Type Stainless-Steel-A1 DIN653
ddkk
M15.50001.5000
M1.26.00001.5000
M1.47.00002.0000
M1.67.50002.0000
M29.00002.0000
M2.511.00002.5000
M312.00002.5000
M416.00003.5000
M520.00004.0000
M624.00005.0000
M830.00006.0000
M1036.00008.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A1
Standard NumberDIN653
Second Standard-
DriveKnurl
HeadROUND
American Generic Brand Term-
Diameter M1,M1.2,M1.4,M1.6,M2,M2.5,M3,M4,M5,M6,M8,M10
Length2,3,4,5,6,,8,10,12,14,16,18,20,22,24,26,28,30,35,40