DDG maxH maxH minW nomF maxF minY 90 deg overY 118 deg short screw
No.100.19000.24700.14800.13400.48000.18800.18001/4" 
1/4"0.25000.33100.19600.17800.62000.25000.24105/16" 
5/16"0.31200.41500.24500.22400.78000.31200.30203/8" 
3/8"0.37500.49700.29300.27000.94000.37500.36207/16" 
7/16"0.43700.58100.34100.31501.09000.43700.42301/2" 
1/2"0.50000.66500.38900.36101.25000.50000.48409/16" 
9/16"0.56200.64800.43700.40701.41000.56200.54505/8" 
5/8"0.65200.83300.48500.45201.56000.62500.60603/4" 
3/4"0.75001.00100.58200.54401.88000.75000.72907/8" 
7/8"0.87501.17000.67800.63502.19000.87500.85201" 
1"1.00001.33700.77400.72602.50001.00000.97401.1/8" 
1.1/8"1.12501.50500.87000.81702.81001.12501.09601.1/4" 
1.1/4"1.25001.67400.96600.90803.12001.25001.21901.1/2" 
1.3/8"1.37501.84301.06301.00003.44001.37501.34201.5/8" 
1.1/2"1.50002.01001.15901.09103.75001.50001.46401.3/4"
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberB18.6.2
Second Standard-
DriveSquare
HeadSquare
American Generic Brand TermTOOL POST
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2"
Length1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10.",11.",12.",13.",14.",15.",16.",17.",18.",19.",20.
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.