UNC Square Head Set Screw Half Dog Pt Case Hardened Steel B18.6.2

SKU: 575
Details
Details
UNC Square Head Set Screw Half Dog Pt Case Hardened Steel B18.6.2
DDG maxP maxP minQH maxH minW nomF maxF min
No.100.19000.24700.12700.12000.04500.14800.13400.48000.18800.1800
1/4"0.25000.33100.15600.14900.06300.19600.17800.62000.25000.2410
5/16"0.31200.41500.20300.19500.07800.24500.22400.78000.31200.3020
3/8"0.37500.49700.25000.24100.09400.29300.27000.94000.37500.3620
7/16"0.43700.58100.29700.28700.10900.34100.31501.09000.43700.4230
1/2"0.50000.66500.34400.33400.12500.38900.36101.25000.50000.4840
9/16"0.56200.64800.39100.37900.14000.43700.40701.41000.56200.5450
5/8"0.65200.83300.46900.45600.15600.48500.45201.56000.62500.6060
3/4"0.75001.00100.56300.54900.18800.58200.54401.88000.75000.7290
7/8"0.87501.17000.65600.64200.21900.67800.63502.19000.87500.8520
1"1.00001.33700.75000.73400.25000.77400.72602.50001.00000.9740
1.1/8"1.12501.50500.84400.82600.28100.87000.81702.81001.12501.0960
1.1/4"1.25001.67400.93800.92000.31200.96600.90803.12001.25001.2190
1.3/8"1.37501.84301.03101.01100.34401.06301.00003.44001.37501.3420
1.1/2"1.50002.01001.12501.10500.37501.15901.09103.75001.50001.4640
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberB18.6.2
Second Standard-
DriveSquare
HeadSquare
American Generic Brand TermTOOL POST
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2"
Length1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8.",8.1/2",9.",9.1/2",10.",11.",12.",13.",14.",15.",16.",17.",18.",19.",20.