Inch Slotted Pan Head Self Tapping Screw B Case Hardened Steel BS4174

SKU: 498
Details
Details
Inch Slotted Pan Head Self Tapping Screw B Case Hardened Steel BS4174
ddk maxdk mink maxk minr nomn maxn mint nom
No.20.16700.15500.05300.04500.03500.03100.02300.0270
No.40.21900.20500.06800.05800.04200.03900.03100.0350
No.60.27000.25600.08200.07200.04600.04800.03900.0440
No.80.32200.30600.09600.08500.05200.05400.04500.0520
No.100.37300.35700.11000.09900.06100.06000.05000.0610
No.120.42500.40700.12500.11200.07800.06700.05600.0690
No.140.49200.47300.14400.13000.08700.07500.06400.0790
No.160.61500.59400.17800.16200.09900.08400.07200.0960
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberBS4174
Second Standard-
DriveSlot
HeadPan
American Generic Brand Term-
Diameter No.2,No.4,No.6,No.8,No.10,No.12,No.14,No.16
Length1/4",5/16",3/8",7/16",1/2",5/8",3/4",1",1.1/4",1.1/2",1.3/4",2",2.1/4",2.1/2",3"