Inch Pozi Pan Head Self Tapping Screw AB Case Hardened Steel BS4174
SKU:
495
Details
Details
Inch Pozi Pan Head Self Tapping Screw AB Case Hardened Steel BS4174
| d | dk max | dk min | k max | k min | r nom |
|---|
| No.2 | 0.1670 | 0.1550 | 0.0620 | 0.0530 | 0.1320 |
| No.4 | 0.2190 | 0.2050 | 0.0800 | 0.0700 | 0.1730 |
| No.6 | 0.2700 | 0.2560 | 0.0970 | 0.0870 | 0.2070 |
| No.8 | 0.3220 | 0.3060 | 0.1150 | 0.1050 | 0.2440 |
| No.10 | 0.3730 | 0.3570 | 0.1330 | 0.1220 | 0.2840 |
| No.12 | 0.4250 | 0.4070 | 0.1510 | 0.1390 | 0.3230 |
| No.14 | 0.4920 | 0.4730 | 0.1750 | 0.1620 | 0.3730 |
| No.16 | 0.6150 | 0.5940 | 0.2180 | 0.2030 | 0.5270 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | CASE HARDENED STEEL |
|---|
| Standard Number | BS4174 |
|---|
| Second Standard | - |
|---|
| Drive | POZI,CROSSRECESS |
|---|
| Head | Pan |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | No.2,No.4,No.6,No.8,No.10,No.12,No.14,No.16 |
|---|
| Length | 1/4",5/16",3/8",7/16",1/2",5/8",3/4",1",1.1/4",1.1/2",1.3/4",2",2.1/4",2.1/2",3" |
|---|