| d | c min | dc max | dc min | k max | k min | s max | smin |
|---|
| St 2.9 | 0.4000 | 6.3000 | 5.8000 | 2.8000 | 2.5000 | 4.0000 | 3.8200 |
| St 3.5 | 0.6000 | 8.3000 | 7.6000 | 3.4000 | 3.0000 | 5.5000 | 5.3200 |
| St 3.9 | 0.6000 | 8.3000 | 7.6000 | 3.4000 | 3.0000 | 5.5000 | 5.3200 |
| St 4.2 | 0.8000 | 8.8000 | 8.1000 | 4.1000 | 3.6000 | 7.0000 | 6.7800 |
| St 4.8 | 0.9000 | 10.5000 | 9.8000 | 4.3000 | 3.8000 | 8.0000 | 7.7800 |
| St 5.5 | 1.0000 | 11.0000 | 10.0000 | 5.4000 | 4.8000 | 8.0000 | 7.7800 |
| St 6.3 | 1.0000 | 13.5000 | 12.2000 | 5.9000 | 5.3000 | 10.0000 | 9.7800 |
| st 8 | 1.2000 | 18.0000 | 16.7000 | 7.0000 | 6.4000 | 13.0000 | 12.7300 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | CASE HARDENED STEEL |
|---|
| Standard Number | DIN6928F |
|---|
| Second Standard | ISO7053 |
|---|
| Drive | Hexagon |
|---|
| Head | Flange |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | St 2.9,St 3.5,St 3.9,St 4.2,St 4.8,St 5.5,St 6.3,st 8 |
|---|
| Length | 6.5,8,10,12,14,16,20,24,25,30,35,40,45,50 |
|---|