Metric Washer Faced Hexagon Head Self Tapping Screw AB Case Hardened Steel DIN6928C

SKU: 447
Details
Details
Metric Washer Faced Hexagon Head Self Tapping Screw AB Case Hardened Steel DIN6928C
dc mindc maxdc mink maxk mins maxsmin
St 2.90.40006.30005.80002.80002.50004.00003.8200
St 3.50.60008.30007.60003.40003.00005.50005.3200
St 3.90.60008.30007.60003.40003.00005.50005.3200
St 4.20.80008.80008.10004.10003.60007.00006.7800
St 4.80.900010.50009.80004.30003.80008.00007.7800
St 5.51.000011.000010.00005.40004.80008.00007.7800
St 6.31.000013.500012.20005.90005.300010.00009.7800
st 81.200018.000016.70007.00006.400013.000012.7300
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberDIN6928C
Second StandardISO7053
DriveHexagon
HeadFlange
American Generic Brand Term-
Diameter St 2.9,St 3.5,St 3.9,St 4.2,St 4.8,St 5.5,St 6.3,st 8
Length6.5,8,10,12,14,16,20,24,25,30,35,40,45,50