Inch Slotted Countersunk Head Self Tapping Screw AB Case Hardened Steel BS4174

SKU: 486
Details
Details
Inch Slotted Countersunk Head Self Tapping Screw AB Case Hardened Steel BS4174
ddk maxdk minkn maxn mint nom
No.20.17200.14700.05100.03100.02300.0190
No.40.22500.19500.06700.03900.03100.0250
No.60.27900.24400.08300.04800.03900.0310
No.80.33200.29200.10000.05400.04500.0370
No.100.38500.34000.11600.06000.05000.0440
No.120.43800.38900.13200.06700.05600.0500
No.140.50700.45200.15300.07500.06400.0580
No.160.63500.56800.19100.08400.07200.0730
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberBS4174
Second Standard-
DriveSlot
HeadCOUNTERSUNK
American Generic Brand TermFLAT
Diameter No.2,No.4,No.6,No.8,No.10,No.12,No.14,No.16
Length1/4",5/16",3/8",7/16",1/2",5/8",3/4",1",1.1/4",1.1/2",1.3/4",2",2.1/4",2.1/2",3"
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.