Inch Unc Sealing Nut

SKU: 1264
Details
Details

 

 

SizeA MaxA MinB Max B MinC
No 2     0.1880     0.1800     0.2170     0.2050     0.0615
No 4     0.2500     0.2410     0.2890     0.2750     0.0925
No 6     0.3120     0.3020     0.3610     0.3440     0.1080
No 8     0.3440     0.3320     0.3970     0.3780     0.1235
No 10     0.3750     0.3620     0.4330     0.4130     0.1235
1/4"     0.5000     0.4880     0.5770     0.5560     0.2340
5/16"     0.5620     0.5460     0.6500     0.6220     0.2960
3/8"     0.6880     0.6690     0.7940     0.7630     0.3590
7/16"     0.7500     0.7280     0.8660     0.8300     0.4210
1/2"     0.8750     0.8500     1.0100     0.9690     0.4840
9/16"     0.9380     0.9090     1.0830     1.0370     0.5460
5/8"     1.0620     1.0310     1.2270     1.1750     0.6090
3/4"     1.2500     1.2120     1.4430     1.3820     0.7340
7/8"     1.4380     1.3940     1.6600     1.5890     0.8590
1"     1.6250     1.5750     1.8760     1.7960     0.9840

 

  Inch Unc Sealing Nut 

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberGRADE 2 AND GRADE 5 AND STAINLESS STEEL
Second Standard-
DriveHexagon
Head-
American Generic Brand Term-
DiameterSEE TABLE
Length.