| Nom Size | Pitch | A Max | A Min | H Max | H Min | Driver size |
| M1.6 | 0.35 | 3.20 | 2.90 | 1.30 | 1.16 | 0 |
| M2 | 0.40 | 4.00 | 3.70 | 1.60 | 1.46 | 0 |
| M2.5 | 0.45 | 5.00 | 4.70 | 2.10 | 1.96 | 1 |
| M3 | 0.50 | 5.90 | 5.30 | 2.40 | 2.26 | 1 |
| M4 | 0.70 | 8.00 | 7.64 | 3.10 | 2.92 | 2 |
| M5 | 0.80 | 9.50 | 9.14 | 3.70 | 3.52 | 2 |
| M6 | 1.00 | 12.00 | 11.57 | 4.60 | 4.30 | 3 |
| M8 | 1.25 | 16.00 | 15.57 | 6.00 | 5.70 | 4 |
| M10 | 1.50 | 20.00 | 19.48 | 7.50 | 7.14 | 4 |
Metric Coarse Phillips Pan Head Seal Screw zago
| Weight | 0.0000 |
|---|---|
| Material | Mild Steel |
| Standard Number | MATERIAL STAINLESS STEEL A2 AND LOW CARBON STEEL |
| Second Standard | - |
| Drive | Phillips |
| Head | Pan |
| American Generic Brand Term | SEAL SCREW |
| Diameter | SEE TABLE |