dM4M5M6M8M10M12M16M20M24
b max5.506.508.8010.8012.1014.1018.5022.5026.50
b min5.006.008.0010.0012.0014.0017.0021.0025.00
c max2.102.102.102.402.903.103.604.105.10
c min1.901.901.902.202.702.903.403.904.70
e max8.7010.2012.2015.2018.2022.2028.2035.3042.30
e min8.309.8011.8014.8017.8021.8027.8034.7041.70
f max3.003.904.606.207.709.2012.7016.2019.20
f min2.803.704.406.007.509.0012.5016.0019.00
g max6.508.009.7511.7514.5016.0020.0025.0030.00
g min6.307.809.5511.5514.3015.8019.8024.8029.80
kmax3.104.104.606.107.709.2011.7014.2017.20
kmin2.903.904.405.907.308.8011.3013.8016.80

 

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN22424
Second Standard-
Drive-
HeadTriangular
American Generic Brand Term-
Diameter0
Length0
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.