SKU: 2295
Details
Details
Metric Coarse Ht Sems Screws with Conical Washer Grade-10.9 DIN69005
dal2 minDIN 6908 hDIN 6908 d2
M2.50.90004.00000.72006.0000
M31.00004.00000.85007.0000
M3.51.20006.00001.06008.0000
M41.40006.00001.30009.0000
M51.60006.00001.550011.0000
M62.00008.00002.000014.0000
M82.500010.00002.600018.0000
M103.000012.00003.200023.0000
M123.500014.00003.950029.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberDIN69005
Second StandardISO10644
DriveVarious
HeadVarious
American Generic Brand Term-
Diameter M2.5,M3,M3.5,M2.5,M3,M3.5,M8,M10,M12
Length12,14,16,18,20,22,24,26,28,30,35,40,45,50