Metric Coarse Triangular Head Screw with Collar Steel DIN22424
Metric Coarse Triangular Head Screw with Collar Steel DIN22424 DIN 22424
| d | M4 | M5 | M6 | M8 | M10 | M12 | M16 | M20 | M24 |
|---|---|---|---|---|---|---|---|---|---|
| b max | 5.50 | 6.50 | 8.80 | 10.80 | 12.10 | 14.10 | 18.50 | 22.50 | 26.50 |
| b min | 5.00 | 6.00 | 8.00 | 10.00 | 12.00 | 14.00 | 17.00 | 21.00 | 25.00 |
| c max | 2.10 | 2.10 | 2.10 | 2.40 | 2.90 | 3.10 | 3.60 | 4.10 | 5.10 |
| c min | 1.90 | 1.90 | 1.90 | 2.20 | 2.70 | 2.90 | 3.40 | 3.90 | 4.70 |
| e max | 8.70 | 10.20 | 12.20 | 15.20 | 18.20 | 22.20 | 28.20 | 35.30 | 42.30 |
| e min | 8.30 | 9.80 | 11.80 | 14.80 | 17.80 | 21.80 | 27.80 | 34.70 | 41.70 |
| f max | 3.00 | 3.90 | 4.60 | 6.20 | 7.70 | 9.20 | 12.70 | 16.20 | 19.20 |
| f min | 2.80 | 3.70 | 4.40 | 6.00 | 7.50 | 9.00 | 12.50 | 16.00 | 19.00 |
| g max | 6.50 | 8.00 | 9.75 | 11.75 | 14.50 | 16.00 | 20.00 | 25.00 | 30.00 |
| g min | 6.30 | 7.80 | 9.55 | 11.55 | 14.30 | 15.80 | 19.80 | 24.80 | 29.80 |
| kmax | 3.10 | 4.10 | 4.60 | 6.10 | 7.70 | 9.20 | 11.70 | 14.20 | 17.20 |
| kmin | 2.90 | 3.90 | 4.40 | 5.90 | 7.30 | 8.80 | 11.30 | 13.80 | 16.80 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | DIN22424 |
| Second Standard | - |
| Drive | - |
| Head | Triangular |
| American Generic Brand Term | - |
| Diameter | 0 |
| Length | 0 |