Metric Coarse 12 Point Socket Screw with Flange Head Grade-12.9 DIN34822
Metric Coarse 12 Point Socket Screw with Flange Head Grade-12.9 DIN34822
| d | M6 | M8 | M10 | M12 | M14 | M16 |
|---|---|---|---|---|---|---|
| dk max | 11.0000 | 14.5000 | 17.0000 | 19.0000 | 22.5000 | 25.5000 |
| dk min | 10.5700 | 14.0700 | 16.5700 | 18.4800 | 21.9800 | 24.9800 |
| dc max | 14.2000 | 18.0000 | 22.3000 | 26.6000 | 30.5000 | 35.0000 |
| dc min | 13.1000 | 16.9000 | 21.0000 | 25.3000 | 28.9000 | 23.4000 |
| k max | 6.0000 | 8.0000 | 10.0000 | 12.0000 | 14.0000 | 16.0000 |
| k min | 5.7000 | 7.6400 | 9.6400 | 11.5700 | 13.5700 | 15.5700 |
| t max | 3.4000 | 4.4800 | 5.4800 | 6.4800 | 7.5800 | 8.5800 |
| t min | 3.0000 | 4.0000 | 5.0000 | 6.0000 | 7.0000 | 8.0000 |
| h max | 4.2000 | 5.4800 | 6.7800 | 8.0800 | 9.4800 | 10.5800 |
| e | 7.4000 | 9.8400 | 11.7000 | 13.5400 | 15.9900 | 17.1800 |
| Drive | N8 | N10 | N12 | N14 | N16 | N18 |
FOR ADDITIONAL DRIVE INFORMATION SEE DIN 34824
Metric Coarse 12 Point Socket Screw with Flange Head Grade 12.9 DIN 34822
| Weight | 0.0000 |
|---|---|
| Material | Grade-12.9 |
| Standard Number | DIN34822 |
| Second Standard | - |
| Drive | 12point |
| Head | Flange |
| American Generic Brand Term | CHEESE,FLANGE,INTERNALFERRY |
| Diameter | M6,M8,M10,M12,M14,M16 |
| Length | 30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200 |