| size | A min | A max | F min | F max | D min | D max | d min | d max | P min | P max | Q min | Q max | drive | R min | R max |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 3.5 | 7.9000 | 8.5000 | 4.5000 | 7.0000 | 3.5000 | 3.9000 | 2.0500 | 2.3500 | 2.7000 | 2.8000 | 2.3500 | 2.9300 | No.2 | 4.5000 | 5.0000 |
| 3.9 | 7.9000 | 8.5000 | 4.5000 | 7.0000 | 3.7000 | 4.0000 | 2.2000 | 2.5000 | 2.7000 | 2.9000 | 2.3500 | 2.9300 | No.2 | 4.5000 | 5.0000 |
| 4.2 | 7.9000 | 8.5000 | 4.5000 | 7.0000 | 4.2000 | 4.6000 | 2.5500 | 2.8500 | 2.8000 | 2.9000 | 2.3500 | 2.9300 | No.2 | 4.5000 | 5.0000 |
| 4.8 | 8.5000 | 9.1000 | 4.5000 | 7.0000 | 4.9000 | 5.3500 | 3.0500 | 3.3500 | 3.1000 | 3.2000 | 2.5000 | 3.1800 | No.2 | 4.5000 | 5.0000 |
Metric Phillips Bugle Head Screw Coarse Thread Hardened Steel
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | . |
| Second Standard | - |
| Drive | Phillips |
| Head | - |
| American Generic Brand Term | - |
| Diameter | 0 |
| Length | 0 |