| d | j max | j min | h max | h min | g min | m max | m min |
|---|
| M4 | 21.0000 | 19.0000 | 11.0000 | 9.0000 | 1.1000 | 4.6000 | 3.2000 |
| M5 | 26.5000 | 24.5000 | 13.0000 | 11.0000 | 1.5000 | 6.0000 | 4.0000 |
| M6 | 32.0000 | 29.0000 | 16.0000 | 14.0000 | 1.5000 | 7.0000 | 5.0000 |
| M8 | 38.0000 | 35.0000 | 19.0000 | 17.0000 | 2.0000 | 8.5000 | 6.5000 |
| M10 | 50.0000 | 47.0000 | 24.0000 | 22.0000 | 3.6000 | 10.0000 | 8.0000 |
| M12 | 66.0000 | 63.0000 | 32.0000 | 29.0000 | 4.1000 | 13.0000 | 10.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A4 |
|---|
| Standard Number | DIN318 |
|---|
| Second Standard | - |
|---|
| Drive | Wing |
|---|
| Head | NON |
|---|
| American Generic Brand Term | THUMB |
|---|
| Diameter | M4,M5,M6,M8,M10,M12 |
|---|
| Length | 6,8,10,16,20,30,35,40,50,60 |
|---|