Metric Coarse Slotted Raised Countersunk Machine Screw with Dog Cone Point Grade-5.8 DIN924

SKU: 311
Details
Details
Metric Coarse Slotted Raised Countersunk Machine Screw with Dog Cone Point Grade-5.8 DIN924
D dk max k max n min t max a dp max l1 min l1 max l2 min l2 max
?1.42.60000.84000.30000.65000.60000.80001.60002.50000.60001.0000
?1.63.00000.96000.40000.80000.70000.80002.00003.00001.00001.6000
?23.80001.20000.50001.00000.80001.20002.50004.00001.00002.0000
?2.54.70001.50000.60001.20000.90001.50003.00005.00001.60002.5000
?35.60001.65000.80001.45001.00002.00004.00006.00001.60003.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-5.8
Standard NumberDIN924
Second Standard-
DriveSlot
HeadRaisedcountersunk
American Generic Brand TermFLAT,OVAL
Diameter M1.4,M1.6,M2,M2.5,M3
Length2,3,4,5,6,8,10,12,14,16,18,20