UNC Phillips Binding Head Machine Screw Grade-4.8 B18.6.3
UNC Phillips Binding Head Machine Screw Grade-4.8 B18.6.3
| d | No. 2 | No.4 | No.6 | No.8 | No.10 | 1/4" |
|---|---|---|---|---|---|---|
| A Max | 0.181 | 0.235 | 0.290 | 0.344 | 0.399 | 0.525 |
| A Min | 0.171 | 0.223 | 0.275 | 0.326 | 0.378 | 0.498 |
| O Max | 0.050 | 0.068 | 0.087 | 0.105 | 0.123 | 0.165 |
| O Min | 0.043 | 0.061 | 0.078 | 0.095 | 0.112 | 0.152 |
| F Max | 0.018 | 0.025 | 0.032 | 0.039 | 0.045 | 0.061 |
| F Min | 0.013 | 0.018 | 0.024 | 0.029 | 0.034 | 0.046 |
| M Max | 0.100 | 0.118 | 0.160 | 0.186 | 0.205 | 0.281 |
| M Min | 0.087 | 0.105 | 0.147 | 0.173 | 0.192 | 0.268 |
| G Max | 0.058 | 0.077 | 0.088 | 0.114 | 0.134 | 0.164 |
| G Min | 0.041 | 0.059 | 0.064 | 0.090 | 0.109 | 0.140 |
| N Min | 0.017 | 0.017 | 0.026 | 0.028 | 0.029 | 0.046 |
| Driver | 1 | 1 | 2 | 2 | 2 | 3 |
UNC Phillips Binding Head Machine Screw Grade CLASS 4.8 4.6 B18.6.3
| Weight | 0.0000 |
|---|---|
| Material | Grade-4.8 |
| Standard Number | B18.6.3 |
| Second Standard | - |
| Drive | - |
| Head | - |
| American Generic Brand Term | - |
| Diameter | 0 |
| Length | 0 |