| d | d max | dk max | dk min | k max | k min | f approx | n max | n min | t nom |
|---|
| 0BA | 0.2360 | 0.4130 | 0.4030 | 0.1670 | 0.1590 | 0.4130 | 0.0640 | 0.0560 | 0.0920 |
| 1BA | 0.2090 | 0.3660 | 0.3560 | 0.1480 | 0.1410 | 0.3660 | 0.0580 | 0.0500 | 0.0810 |
| 2BA | 0.1850 | 0.3190 | 0.3090 | 0.1300 | 0.1230 | 0.3090 | 0.0520 | 0.0440 | 0.0710 |
| 3BA | 0.1610 | 0.2830 | 0.2730 | 0.1130 | 0.1070 | 0.2830 | 0.0470 | 0.0390 | 0.0620 |
| 4BA | 0.1420 | 0.2520 | 0.2420 | 0.1010 | 0.0950 | 0.2520 | 0.0400 | 0.0340 | 0.0560 |
| 5BA | 0.1260 | 0.2210 | 0.2110 | 0.0880 | 0.0830 | 0.2210 | 0.0400 | 0.0340 | 0.0480 |
| 6BA | 0.1100 | 0.1940 | 0.1840 | 0.0780 | 0.0730 | 0.1940 | 0.0330 | 0.0270 | 0.0430 |
| 7BA | 0.0980 | 0.1730 | 0.1630 | 0.0690 | 0.0640 | 0.1730 | 0.0330 | 0.0270 | 0.0380 |
| 8BA | 0.0870 | 0.1570 | 0.1470 | 0.0630 | 0.0590 | 0.1570 | 0.0300 | 0.0240 | 0.0350 |
| 9BA | 0.0750 | 0.1280 | 0.1230 | 0.0530 | 0.0480 | 0.1280 | 0.0300 | 0.0240 | 0.0290 |
| 10BA | 0.0670 | 0.1120 | 0.1070 | 0.0450 | 0.0410 | 0.1120 | 0.0240 | 0.0190 | 0.0250 |
| 11BA | 0.0590 | 0.1100 | 0.1050 | 0.0450 | 0.0410 | 0.1100 | 0.0240 | 0.0190 | 0.0250 |
| 12BA | 0.0510 | 0.0950 | 0.0900 | 0.0380 | 0.0350 | 0.0950 | 0.0200 | 0.0150 | 0.0210 |
| 13BA | 0.0470 | 0.0810 | 0.0760 | 0.0320 | 0.0290 | 0.0810 | 0.0200 | 0.0150 | 0.0180 |
| 14BA | 0.0390 | 0.0640 | 0.0590 | 0.0260 | 0.0230 | 0.0640 | 0.0150 | 0.0110 | 0.0140 |
| 15BA | 0.0350 | 0.0640 | 0.0590 | 0.0260 | 0.0230 | 0.0640 | 0.0150 | 0.0110 | 0.0140 |
| 16BA | 0.0310 | 0.0580 | 0.0540 | 0.0230 | 0.0200 | 0.0580 | 0.0130 | 0.0090 | 0.0130 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Grade-4.8 |
|---|
| Standard Number | BS57 |
|---|
| Second Standard | - |
|---|
| Drive | Slotted |
|---|
| Head | ROUND |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | 0BA,1BA,2BA,3BA,4BA,5BA,6BA,7BA,8BA,9BA,10BA,11BA,12BA,13BA,14BA,15BA,16BA |
|---|
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2." |
|---|
Reviews
Tags