Metric Coarse Slotted Pan Head Machine Screw Nylon-66 DIN85

SKU: 372
Details
Details
Metric Coarse Slotted Pan Head Machine Screw Nylon-66 DIN85
d1tnkdk
M2 0.50001.30004.0000
M2.5 0.60001.50005.0000
M30.70000.80001.80006.0000
M3.50.80001.00002.10007.0000
M41.00001.20002.40008.0000
M51.20001.20003.000010.0000
M61.40001.60003.600012.0000
M81.90002.00004.800016.0000
M102.40002.50006.000020.0000
Additional Info
Additional Info
Weight0.0000
MaterialNylon-66
Standard NumberDIN85
Second StandardISO1580
DriveSlot
HeadPan
American Generic Brand Term-
Diameter M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10
Length2,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60