BSF Slotted Pan Head Machine Screw Grade-4.8 BS450
| d | d | dk max | dk min | k max | k min | n max | n min | t nom |
|---|---|---|---|---|---|---|---|---|
| 1/8” | 0.1250 | 0.2450 | 0.2310 | 0.0750 | 0.0650 | 0.0390 | 0.0320 | 0.0400 |
| 3/16” | 0.1875 | 0.3730 | 0.3570 | 0.1100 | 0.0990 | 0.0500 | 0.0420 | 0.0610 |
| 7/32” | 0.2188 | 0.4250 | 0.4070 | 0.1250 | 0.1120 | 0.0550 | 0.0460 | 0.0690 |
| 1/4” | 0.2500 | 0.4920 | 0.4730 | 0.1440 | 0.1300 | 0.0610 | 0.0510 | 0.0780 |
| 5/16” | 0.3125 | 0.6150 | 0.5940 | 0.1780 | 0.1620 | 0.0710 | 0.0610 | 0.0950 |
| 3/8” | 0.3750 | 0.7400 | 0.7160 | 0.2120 | 0.1950 | 0.0820 | 0.0720 | 0.1120 |
| 7/16” | 0.4375 | 0.8630 | 0.8380 | 0.2470 | 0.2270 | 0.0930 | 0.0820 | 0.1290 |
| 1/2” | 0.5000 | 0.9870 | 0.9580 | 0.2810 | 0.2600 | 0.1040 | 0.0920 | 0.1450 |
| 9/16” | 0.5625 | 1.0310 | 0.9990 | 0.3150 | 0.2930 | 0.1150 | 0.1030 | 0.1620 |
| 5/8” | 0.6250 | 1.1250 | 1.0900 | 0.3500 | 0.3250 | 0.1260 | 0.1130 | 0.1790 |
| 3/4” | 0.7500 | 1.2500 | 1.2090 | 0.4190 | 0.3900 | 0.1480 | 0.1340 | 0.2130 |
| Weight | 0.0000 |
|---|---|
| Material | Grade-4.8 |
| Standard Number | BS450 |
| Second Standard | - |
| Drive | Slot |
| Head | Pan |
| American Generic Brand Term | - |
| Diameter | 1/8”,3/16”,7/32”,1/4”,5/16”,3/8”,7/16”,1/2”,9/16”,5/8”,3/4” |
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5." |