D dk k n t a dp l1 min l1 max l2 min l2 max
M1.42.60000.84000.30000.40000.60000.80001.60002.50000.60001.0000
M1.63.00000.96000.40000.45000.70000.80002.00003.00001.00001.6000
M23.80001.20000.50000.60000.80001.20002.50004.00001.00002.0000
M2.54.70001.50000.60000.70000.90001.50003.00005.00001.60002.5000
M35.60001.65000.80000.85001.00002.00004.00006.00001.60003.0000