BSW Whitworth Slotted Round Head Machine Screw Brass BS450
| d | d | dk max | dk min | k max | k min | f nom | n max | n min | t nom |
|---|---|---|---|---|---|---|---|---|---|
| 1/8” | 0.1250 | 0.2190 | 0.2060 | 0.0870 | 0.0820 | 0.2190 | 0.0390 | 0.0320 | 0.0480 |
| 3/16” | 0.1875 | 0.3280 | 0.3120 | 0.1310 | 0.1240 | 0.3280 | 0.0500 | 0.0420 | 0.0720 |
| 7/32” | 0.2188 | 0.3830 | 0.3650 | 0.1530 | 0.1450 | 0.3830 | 0.0550 | 0.0460 | 0.0840 |
| 1/4” | 0.2500 | 0.4380 | 0.4170 | 0.1750 | 0.1650 | 0.4380 | 0.0610 | 0.0510 | 0.0960 |
| 5/16” | 0.3125 | 0.5470 | 0.5240 | 0.2190 | 0.2070 | 0.5470 | 0.0710 | 0.0610 | 0.1200 |
| 3/8” | 0.3750 | 0.6560 | 0.6290 | 0.2620 | 0.2490 | 0.6560 | 0.0820 | 0.0720 | 0.1440 |
| 7/16” | 0.4375 | 0.7660 | 0.7350 | 0.3060 | 0.2910 | 0.7660 | 0.0930 | 0.0820 | 0.1680 |
| 1/2” | 0.5000 | 0.8750 | 0.8400 | 0.3500 | 0.3330 | 0.8750 | 0.1040 | 0.0920 | 0.1920 |
| 9/16” | 0.5625 | 0.9840 | 0.9460 | 0.3940 | 0.3750 | 0.9840 | 0.1150 | 0.1030 | 0.2170 |
| 5/8” | 0.6250 | 1.0940 | 1.0510 | 0.4370 | 0.4170 | 1.0940 | 0.1260 | 0.1130 | 0.2400 |
| 3/4” | 0.7500 | 1.3120 | 1.2620 | 0.5250 | 0.5000 | 1.3120 | 0.1480 | 0.1340 | 0.2880 |
| Weight | 0.0000 |
|---|---|
| Material | BRASS |
| Standard Number | BS450 |
| Second Standard | - |
| Drive | Slotted |
| Head | ROUND |
| American Generic Brand Term | - |
| Diameter | 1/8”,3/16”,7/32”,1/4”,5/16”,3/8”,7/16”,1/2”,9/16”,5/8”,3/4” |
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5." |