BSW Whitworth Slotted Mushroom Head Machine Screw Grade-4.8 BS450
| d | d | dk max | dk min | k max | k min | n max | n min | t nom |
|---|---|---|---|---|---|---|---|---|
| 1/8” | 0.1250 | 0.2890 | 0.2720 | 0.0780 | 0.0660 | 0.0430 | 0.0350 | 0.0400 |
| 3/16” | 0.1875 | 0.4480 | 0.4250 | 0.1180 | 0.1030 | 0.0600 | 0.0500 | 0.0610 |
| 1/4” | 0.2500 | 0.5730 | 0.5460 | 0.1500 | 0.1330 | 0.0750 | 0.0640 | 0.0790 |
| 5/16” | 0.3125 | 0.6980 | 0.6660 | 0.1830 | 0.1620 | 0.0840 | 0.0720 | 0.0960 |
| 3/8” | 0.3750 | 0.8230 | 0.7870 | 0.2150 | 0.1910 | 0.0940 | 0.0810 | 0.1120 |
| Weight | 0.0000 |
|---|---|
| Material | Grade-4.8 |
| Standard Number | BS450 |
| Second Standard | - |
| Drive | Slot |
| Head | Mushroom |
| American Generic Brand Term | TRUSS,SHALLOW PAN, MUSHROOM |
| Diameter | 1/8”,3/16”,7/32”,1/4”,5/16”,3/8” |
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5." |