BSF Slotted Raised Cheese Head Machine Screw Grade-4.8 BS450
| d | d | dk max | dk min | k nom | b max | b min |
|---|---|---|---|---|---|---|
| 1/8” | 0.1250 | 0.2050 | 0.1870 | 0.0830 | 0.1200 | 0.1000 |
| 3/16” | 0.1875 | 0.3130 | 0.2920 | 0.1240 | 0.1800 | 0.1560 |
| 7/32” | 0.2188 | 0.3570 | 0.3340 | 0.1420 | 0.2050 | 0.1780 |
| 1/4” | 0.2500 | 0.4140 | 0.3890 | 0.1630 | 0.2370 | 0.2070 |
| 5/16” | 0.3125 | 0.5180 | 0.4900 | 0.1990 | 0.2950 | 0.2620 |
| 3/8” | 0.3750 | 0.6220 | 0.5900 | 0.2600 | 0.3550 | 0.3150 |
| 7/16” | 0.4375 | 0.6250 | 0.5890 | 0.2840 | 0.3680 | 0.3210 |
| 1/2” | 0.5000 | 0.7500 | 0.7100 | 0.3110 | 0.4120 | 0.3620 |
| Weight | 0.0000 |
|---|---|
| Material | Grade-4.8 |
| Standard Number | BS450 |
| Second Standard | - |
| Drive | Pozi, Cross Recess |
| Head | RAISEDCHEESE |
| American Generic Brand Term | FILLISTER |
| Diameter | 1/8”,3/16”,7/32”,1/4”,5/16”,3/8”,7/16”,1/2” |
| Length | 1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5." |