BA Slotted Countersunk Head Machine Screw Grade-4.8 BS57
dd maxdk maxdk mink nomn maxn mint nom
0BA0.23600.41300.40300.09900.06400.05600.0450
1BA0.20900.36600.35600.08900.05800.05000.0410
2BA0.18500.31900.30900.07700.05200.04400.0360
3BA0.16100.28300.27300.07100.04700.03900.0330
4BA0.14200.25200.24200.06500.04000.03400.0310
5BA0.12600.22100.21100.05800.04000.03400.0280
6BA0.11000.19400.18400.05100.03300.02700.0240
7BA0.09800.17300.16300.04700.03300.02700.0230
8BA0.08700.15700.14700.04300.03000.02400.0210
9BA0.07500.12800.12300.03500.03000.02400.0180
10BA0.06700.11200.10700.03000.02400.01900.0160
11BA0.05900.11000.10500.03300.02100.01900.0160
12BA0.05100.09500.09000.02800.02000.01500.0140
13BA0.04700.08100.07600.02300.02000.01500.0120
14BA0.03900.06400.05900.01900.01500.01100.0110
15BA0.03500.06400.05900.02100.01500.01100.0110
16BA0.03100.05800.05400.01900.01300.00900.0100
Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.8
Standard NumberBS57
Second Standard-
DriveSlot
HeadCOUNTERSUNK
American Generic Brand TermFLAT
Diameter 0BA,1BA,2BA,3BA,4BA,5BA,6BA,7BA,8BA,9BA,10BA,11BA,12BA,13BA,14BA,15BA,16BA
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2."