dd maxdk maxdk mink nom
0BA0.23600.41300.40300.0990
1BA0.20900.36600.35600.0890
2BA0.18500.31900.30900.0770
3BA0.16100.28300.27300.0710
4BA0.14200.25200.24200.0650
5BA0.12600.22100.21100.0580
6BA0.11000.19400.18400.0510
7BA0.09800.17300.16300.0470
8BA0.08700.15700.14700.0430
9BA0.07500.12800.12300.0350
10BA0.06700.11200.10700.0300
11BA0.05900.11000.10500.0330
12BA0.05100.09500.09000.0280
13BA0.04700.08100.07600.0230
14BA0.03900.06400.05900.0190
15BA0.03500.06400.05900.0210
16BA0.03100.05800.05400.0190
Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.8
Standard NumberBS57
Second Standard-
DrivePozi, Cross Recess
HeadCOUNTERSUNK
American Generic Brand TermFLAT
Diameter 0BA,1BA,2BA,3BA,4BA,5BA,6BA,7BA,8BA,9BA,10BA,11BA,12BA,13BA,14BA,15BA,16BA
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2."