Metric Fine Hexagon Head Set Screw Fine Pitch Stainless-Steel-A2 DIN961
| d | k | e | s |
|---|---|---|---|
| M6(0.75p) | 4.0000 | 11.0500 | 10.0000 |
| M8(1.00p) | 5.3000 | 14.3800 | 13.0000 |
| M10(1.00p) | 6.4000 | 18.9000 | 17.0000 |
| M10(1.25P) | 6.4000 | 18.9000 | 17.0000 |
| M12(1.25p) | 7.5000 | 21.1000 | 19.0000 |
| M12(1.50p) | 7.5000 | 21.1000 | 19.0000 |
| M14(1.5p) | 8.8000 | 24.4900 | 22.0000 |
| M16(1.5p) | 10.0000 | 26.7500 | 24.0000 |
| M18(1.5P) | 11.5000 | 27.0000 | |
| M20(1.5P) | 12.5000 | 30.0000 | |
| M24(2.0P) | 15.0000 | 36.0000 | |
| M27(2.00P) | 17.0000 | 41.0000 |
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel-A2 |
| Standard Number | DIN961 |
| Second Standard | ISO8676 |
| Drive | Hexagon |
| Head | HEXAGON |
| American Generic Brand Term | TAPBOLT |
| Diameter | M6(0.75p),M8(1.00p),M10(1.00p),M10(1.25P),M12(1.25p),M12(1.50p),M14(1.5p),M16(1.5p),M18(1.5P),M20(1.5P),M24(2.0P),M27(2.00P) |
| Length | 6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100 |